Fatigue crack initiation and propagation in plain and notched PBF-LB/M, WAAM, and wrought 316L stainless steel specimens

Chronological data

Date of first publication2024-07-10
Date of publication in PubData 2026-10-14

Language of the resource

English

Related external resources

Variant form of DOI : 10.1016/j.matdes.2024.113122
Braun, M., Chen, T., Shen, J., Fassmer, H., Klusemann, B., Sheikhi, S., Ehlers, S., Müller, E., Sarmast, A., & Schubnell, J. (2024). Fatigue crack initiation and propagation in plain and notched PBF-LB/M, WAAM, and wrought 316L stainless steel specimens. Materials & Design, 244, Article 113122.
Published in ISSN : 0264-1275
Materials & Design

Abstract

Additively manufactured (AM) components—either made by laser-powder bed fusion or wire and arc additive manufacturing—typically contain process-related defects on and near surfaces that can be removed by machining. Various studies have shown that post-treatment, such as machining significantly improves the fatigue strength of AM parts. To this day, however, hardly any studies have investigated the fatigue strength of post-treated additively manufactured components with notches. In this study, fatigue tests were performed on plain and notched specimens to determine and compare the crack initiation and crack propagation behavior due to different manufacturing-related effects. Tests were performed on specimens produced by the two aforementioned AM processes and compared to specimens taken from wrought sheets. The fatigue strength of AM materials is influenced by microstructure, defects, residual stress, and notches. PBF-LB/M specimens exhibit the highest fatigue strength in plain, notch-free conditions, attributed to differences in microstructure and static strength affecting fatigue crack initiation. Notched specimens show larger differences among materials, with PBF-LB/M having shorter fatigue crack propagation life related to line-type defect clusters, while the plain PBF-LB/M specimens are less affected as their fatigue strength is primarily determined by fatigue crack initiation.

Keywords

Hybrid Additive Manufacturing; Selective Laser Melting; Wire Arc Additive Manufacturing; Microstructural Defect; Post-production Treatment; Fatigue Strength Assessment